Specification DN | Outside diameter dem/mm | Wall thickness and tolerance mm | Out-of-roundness % | |||
Nominal value | Tolerance | Standard Value | Tolerance | Before Coiling | After Coiling | |
32/26 | 32 | 0.3 | 2.5 | 0.3 | ≤2 | ≤3 |
0 | 0 | |||||
34/28 | 34 | 0.3 | 3 | 0.3 | ≤2 | ≤3 |
0 | 0 | |||||
40/33 | 40 | 0.4 | 3.5 | 0.35 | ≤2.5 | ≤3.5 |
0 | 0 | |||||
46/38 | 46 | 0.4 | 4 | 0.35 | ≤3 | ≤5 |
0 | 0 | |||||
50/41 | 50 | 0.5 | 4.5 | 0.4 | ≤3 | ≤5 |
0 | 0 | |||||
63/54 | 63 | 0.6 | 5 | 0.4 | ≤3 | ≤5 |
0 | 0 | |||||
The specification dimensions and tolerances of ribbed pipes shall be determined through negotiation between the supplier and the buyer. | ||||||



Physical and chemical properties of HDPE silicon core tube GB/T24456-2009 | ||||||
Item | 32/26 | 34/28 | 40/33 | 46/38 | 50/41 | 63/54 |
Outer wall hardness/HD | ≥59 | |||||
Inner wall friction coefficient | static state ≤0.25 Plate method, standard test rod for PE-HD | |||||
dynamic condition ≤0.15Round drum method | ||||||
Tensile yield strength/MPa | ≥20 | |||||
Elongation at break/% | ≥500 | |||||
Maximum traction load/N | ≥5000 | ≥6000 | ≥8000 | ≥10000 | ≥11000 | ≥12000 |
Cold bending property | According to the bending radius below, the silicon core tube of the corresponding specifications should be cold bending test, there should be no cracking and obvious stress whitening phenomenon. | |||||
300mm | 300mm | 400mm | 500mm | 625mm | 750mm | |
Ring-stiffness/ kN/Squre Meter | ≥50 | ≥40 | ≥30 | |||
Recovery rate/% | When the deformation of the outer diameter is 50% of the original outer diameter under vertical pressure, it is immediately unloaded, the pattern is not broken and not stratified, and the inner and outer diameter can naturally recover to more than 85% of the original in 10min. | |||||
Resistance to drop hammer impact | At a temperature of -20°C, impact 10 samples with 15.3Kg weight hammer, and more than 9 (including) should pass through | |||||
Hydraulic resistance | Under the condition of temperature 20°C and water pressure 2.0MPa, the sample was kept for 15min, and no visible cracks or cracks were detected. | |||||
Longitudinal shrinkage ratio/% | ≤3.0 | |||||
Resistance to environmental stress cracking | 48 hours, failure number ≤20% | |||||
Resistance to hydrocarbons | After soaking with heptane for 720h, 528N external force is applied to the silicon core tube, the sample is not damaged, and the permanent deformation is not more than 5%. | |||||